You can see where around corners and even some straight runs it is peeling up. I’m running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I’ve trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

  • BingoBangoBongo@midwest.socialOP
    link
    fedilink
    English
    arrow-up
    0
    ·
    10 months ago

    I was able to get it printing, but doing some calibration confirms that adjusting z offset made the bottom layer better. What’s the point in z offset specifically, vs just changing the gap when tramming or the initial layer height?