Ok guys, I’m breaking down and posting here to see if anyone has any ideas. I’m greatful for any advice.
I have an upgraded flsun SR. I recently lost my computer (psu issue, waiting for replacement) and I took this opportunity to switch from Cura to Orcaslicer.
Over-all I’m very happy, and getting some good speeds, but I just cannot remove stringing no matter what I try:
- Retraction from 0-7mm. After about 3mm, no further effect
- Retraction speed from 30mm/s-50mm/s. No noticable effect
- Travel speed and acceleration both high (up to 350mm/s and 6000 accel. No effect
- Temp from 205-215 with no effect
- Dried filament and different colours, no effect
- Wipe on retract on and off, up to 2mm wipe distance and 100% retraction. No effect
- Messed with scarf seams on and off, no effect
- No effect from layer heights
My setup:
- Printer - FLSun SR running klipper with a speede pad
- Filament - Esun PLA+
- Upgrades - Deported fans, OMG v2 extruder, volcano hotend and high flow cht nozzle
Removed by mod
Hey mate, I keep my filament in a dry cabinet at 5ish% humidity, and I’ve had the same results with two different filaments in there. I even chucked my filament in a food dehydrator at 40C for 12h with no effect. I’m pretty sure the filament is dry!
Removed by mod
It’s all good mate! Thanks for the suggestion. When I first started printing I had that exact issue.